rusty_apache

The process works best in the heat of direct sunlight. I treat the parts with metal prep right out the vat. Then it is rinsed and quick dried with compressed air and then a heat gun if the sun's not out. Then it's ready for paint or plating.

The best thing about it that you can leave it boiling for a long time and it doesn't attack the metal itself


From the category:

Mechanical

· 88 images
  • 88 images
  • 2 image comments

Photo Information

  • Taken with NIKON CORPORATION NIKON D3100
  • Focal Length 18 mm
  • Exposure Time 10/4000
  • f Aperture f/5.0
  • ISO Speed 100

Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

We have placed cookies on your device to help make this website better. You can adjust your cookie settings, otherwise we'll assume you're okay to continue.

Terms of Use